Test Online Free API API-570 Exam Questions and Answers
The questions for API-570 were last updated On Nov.30 2022 Get API-570 Full AccessQuestion No : 1
An operator notice a pipe off its support, what should be done?
Answer:
Question No : 2
A piping system started with a wall thickness of 0.375 inches. Over a five year period the wall thickness is now 0.1”.
What is the long term corrosion rate?
Answer:
Question No : 3
The weld ripples of reinforcement of butt-welded joints shall be before radiography.
Answer:
Question No : 4
Temperatures above can damage transducers not equipped with delay line material.
Answer:
Question No : 5
Of the following examples, which one may cause a leak in a threaded joint?
Answer:
Question No : 6
During a welder qualification test on 3/8” plate in the horizontal position, how many guided bends are required?
Answer:
Question No : 7
Besides ultrasonic instruments, what other method can be used to determine thickness measurements?
Answer:
Question No : 8
Aboveground piping is subject to atmospheric corrosion.
What is buried piping subject to?
Answer:
Question No : 9
Why should a leaking threaded joint not be tightened while the system is in service?
Answer:
Question No : 10
03 inches/year 5 Years
MAWP:
Answer: